Thickness 3700 - 4300 microns
146 - 169 mil
Standard
Parker Chomerics WIN-SHIELD™ Elite EMI Shielded Window
Description: Shielded Windows WIN-SHIELD™ EMI shielded windows provide exceptional optical performance without sacrificing EMI shielding. This new generation of shielded windows is designed specif..
Thickness 3700 microns
146 mil
Sheet; Internal
Azdel Plus R451-B02 45% Continuous Random Fiber Mat / PP Resin Matrix
AZDEL® R451-B01 is a glass mat thermoplastic laminate based upon a random oriented continuous fiber mat contained within a polypropylene resin matrix. This composite material features high flow pr..
Thickness 3700 microns
146 mil
Sheet; Internal
Azdel Plus R401-B01 40% Continuous Random Fiber Mat / PP Resin Matrix
AZDEL® R401-B01 is a glass mat thermoplastic laminate based upon a random oriented continuous fiber mat contained within a polypropylene resin matrix. This composite material features high flow pr..