Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 14000 - 92000 microns | 551 - 3620 mil | intermediate sizes also available |
Superior Die Set FORTAL® HR Aluminum Alloy Description: FORTAL is a high strength, lightweight, easy to machine alloy, originally developed to be used in the aerospace industry. It can be found whenever a structure is highly solicited and d.. |