Thickness 920.0 microns
36.22 mil
Average
Daikin POLYFLON PA-10L PTFE Paper
Papers made from POLYFLON PTFE papers are manufactured from POLYFLON PTFE fibrous powder, and do not contain any other substances. This paper is soft, elastic, and has very low gas permeability. P..