Physical Properties Metric English Comments
Thickness 36.0 microns
1.42 mil
Dry Recommended Film
Chesterton 740 Heavy Duty Rust Guard
Description: Chesterton® 740 Heavy Duty Rust Guard is a premium quality corrosion preventative coating designed with user ease of application in mind. It is the perfect coating for those areas of t..