Polymer Property : Thickness = 35000 microns Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Thickness 35000 microns
1378 mil
Zircar Refractory Composites RSMAT-3000 ALUMINA MAT
ZRCI Type RSMAT-3000 is a high purity, high temperature, flexible form composed of continuous 97% alumina ceramic fibers designed for use to 1650°C (3002°F). Type RSMAT-3000 contains little shot a..