Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 840 microns | 33.1 mil | 120 |
LATI Latigray 53/22-01 CX/70 PP Homopolymer, Impact Modified Radiopaque compound based on Polypropylene homopolymer (PPh), impact modified. Special mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformati.. |