Physical Properties Metric English Comments
Thickness 810 microns
31.9 mil
Standard; Laminate
GrafTech GRAFOIL® GHR Standard Fluid Sealing Laminate, Metal Reinforced
GRAFOIL® Grade GHR is an uncured laminate made with GRAFOIL® Grade GTB flexible graphite adhesively bonded to both faces of a 0.002" thick flat 316 or 316L stainless steel insert. Surface iden..