Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 307 microns | 12.1 mil | ASTM D3652 |
3M 8979 Performance Plus Duct Tape 3M™ Performance Plus Duct Tape 8979 has a unique product construction for indoor and outdoor applications. This tape is removable with little or no adhesive residue from most opaque surfaces up to .. |
|||
Thickness | 307 microns | 12.1 mil | ASTM D3652 |
3M 8979N Performance Plus Duct Tape Nuclear Grade 3M™ Performance Plus Duct Tape 8979N has a unique product construction for indoor and outdoor applications. This tape is removable with little or no adhesive residue from most opaque surfaces up to.. |