Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 254 - 305 microns | 10.0 - 12.0 mil | Overall |
Arlon R31901R011 0.011" (0.279 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place.. |
|||
Thickness | 254 - 305 microns | 10.0 - 12.0 mil | Overall |
Arlon R34931R010 0.011" (0.279 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place .. |
|||
Thickness | 254 - 305 microns | 10.0 - 12.0 mil | Overall |
Arlon 44571B010 0.011" (0.279 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone Rubber This data represents typical values for the production material. The data should not be used to write, or in place.. |
|||
Thickness | 254 - 305 microns | 10.0 - 12.0 mil | Overall |
Arlon 44571R010 0.011" (0.279 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass clothThis data represents typical values for the production material. T.. |
|||
Thickness | 229 - 305 microns | 9.00 - 12.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 49091R010 0.0105" (0.267 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured RubberSide 2: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass fabricThis data Represents typical values for the production material. The data s.. |
|||
Thickness | 229 - 305 microns | 9.00 - 12.0 mil | Overall |
Arlon 912-10RXX-P0 0.012" (0.305 mm) Self-Fusing Silicone Tape Design/Construction:Cross Section Type: RectangularArlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tape is not required.P.. |