Polymer Property : Thickness = 3.24 mil Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Thickness 82.3 microns
3.24 mil
estimated wet film thickness
Aremco Quartz-Coat™ 845 High Temperature Ceramic-Inorganic Coating
Single part, waterborne, silicon-filled, phosphate-bonded, brown-black coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps..