Physical Properties Metric English Comments
Thickness 3.05 microns
0.120 mil
Arlon AD450A Glass, PTFE and Ceramic
High Dielectric Constant for Circuit Militarization & Patch Antenna ApplicationsInformation provided by Arlon Materials for Electronics (MED).