Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 23810 - 26990 microns | 937.5 - 1063 mil | Width |
Arlon 912-10R12-P1 0.012" (0.305 mm) Self-Fusing Silicone Tape Design/Construction:Cross Section Type: RectangularRoll Length: 12 Yards Width, inches: 1Arlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth.. |
|||
Thickness | 23810 - 26990 microns | 937.5 - 1063 mil | Width |
Arlon LW201Xxx-M1 0.020" (0.508 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) with Mylar Interleave Design/Construction:Cross Section Type: TriangularArlon LevelWrap® Tape: LevelWrap® has tapered edges and a colored line along its apes. The purpose of the line is to act as a guide for subsequent.. |
|||
Thickness | 23810 - 26990 microns | 937.5 - 1063 mil | Width |
Arlon LW201Xxx-P0 0.020" (0.508 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) with Poly Interleave Design/Construction:Triangular Cross Section Fusible TapeArlon LevelWrap® Tape: LevelWrap® has tapered edges and a colored line along its apes. The purpose of the line is to act as a guide for sub.. |
|||
Thickness | 23810 - 26990 microns | 937.5 - 1063 mil | Width |
Arlon LW201Xxx-P1 0.020" (0.508 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) with Poly Interleave Design/Construction:Triangular Cross Section Fusible TapeArlon LevelWrap® Tape: LevelWrap® has tapered edges and a colored line along its apes. The purpose of the line is to act as a guide for sub.. |
|||
Thickness | 23810 - 26990 microns | 937.5 - 1063 mil | Width |
Arlon LW301Rxx-P1 0.030" (0.762 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) with Poly Interleave Design/Construction:Triangular Cross Section Fusible TapeArlon LevelWrap® Tape: LevelWrap® has tapered edges and a colored line along its apes. The purpose of the line is to act as a guide for sub.. |
|||
Thickness | 23810 - 26990 microns | 937.5 - 1063 mil | Width |
Arlon 912-10C16.4FR-P0 0.012" (0.305 mm) Self-Fusing Silicone Tape Design/Construction:Cross Section Type: RectangularRoll Length: 16.4 Yards Width, inches: 1Arlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smoo.. |
|||
Thickness | 23810 - 26990 microns | 937.5 - 1063 mil | Width |
Arlon LW301Rxx-P0 0.030" (0.762 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) with Poly Interleave Design/Construction:Triangular Cross Section Fusible TapeArlon LevelWrap® Tape: LevelWrap® has tapered edges and a colored line along its apes. The purpose of the line is to act as a guide for sub.. |