Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 208 microns | 8.20 mil | Total; ASTM D3752 |
3M 5453 PTFE Glass Cloth Tape 3M™ PTFE Glass Cloth Tape 5453 has a silicone adhesive which provides a high temperature release surface for protection and insulation.Information provided by 3M |
|||
Thickness | 208 microns | 8.20 mil | |
Hexcel® HexForce™ 341 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |