Polymer Property : Thickness = 20000 microns Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Thickness 20000 - 200000 microns
787 - 7870 mil
With Foil or C/C
Sinotek Materials Rigid Graphite Felt Board Heat Insulation Material
Information provided by Sinotek
Thickness <= 20000 microns
<= 787 mil
Sinotek Materials Graphite Felt Heat Insulation Material
Information provided by Sinotek