Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 20.8 microns | 0.820 mil | Nominal; ExxonMobil Method |
ExxonMobil Bicor® 85 AXT OPP Film Product Description: Bicor ASB-X is a two side coated, sealable OPP film delivering an advanced level of moisture and oxygen battier protection. This film is designed for use in (unsupported and sur.. |