Polymer Property : Thickness = 2.60 mil Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Thickness 55.9 - 66.0 microns
2.20 - 2.60 mil
Cured ply, Typical
Renegade Materials Corporation MVK-14 Polyimide FreeForm™ Astroquartz 4581 Fabric
MVK-14 Polyimide Astroquartz and S2 glass prepregs are an affordable, easy-to-process material for high-temperature radome and antenna applications. MVK-14 is a non-MDA alternative to BMI, cyanate e..
Thickness 55.9 - 66.0 microns
2.20 - 2.60 mil
Cured ply, Typical
Renegade Materials Corporation MVK-14 Polyimide FreeForm™ S2-Glass Fabric
MVK-14 Polyimide Astroquartz and S2 glass prepregs are an affordable, easy-to-process material for high-temperature radome and antenna applications. MVK-14 is a non-MDA alternative to BMI, cyanate e..