Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 1.00 - 2.40 microns | 0.0394 - 0.0945 mil | |
Dow CYCLOTENE™ 3022-35 Bisbenzocyclobutene (BCB) Electronic Resin This product was developed for use as spin-on dieletric materials in microelectronic fabrication.Information provided by Dow |