Polymer Property : Thickness = 18.3 microns Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Thickness 18.3 microns
0.720 mil
Honeywell Capran® Emblem™ 1530 PVDC-Coated Bi-Axially Oriented Nylon Film  (discontinued **)
Capran® Emblem™ 1530 is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hydrocarbons, and many ..