Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 460 microns | 18.1 mil | |
3M Nextel™ AP-18 Woven Tape 312 (2.5 cm) Information provided by 3M |
|||
Thickness | 460 microns | 18.1 mil | |
3M Nextel™ AP-18 Woven Tape 312 (3.8 cm) Information provided by 3M |
|||
Thickness | 460 microns | 18.1 mil | |
3M Nextel™ AP-18 Woven Tape 312 (5.1 cm) Information provided by 3M |