Thickness <= 17000 microns
<= 669 mil
wide range available
Schott B270â„¢ Sheet Glass
B 270â„¢ crown glass in sheet glass form. Manufactured by the up-draw method, offers high stability with respect to solarization in combination with high transmission in the visible wavelength ra..
Thickness <= 17000 microns
<= 669 mil
Trimay® Wear Plate T156 Iron-based Steel Overlay
Overlay Description: T156 is a iron-based steel overlay wear solution with a unique proprietary chemical composition designed for moderate wear environments with moderate impact. T156 is similar to ..
Thickness <= 17000 microns
<= 669 mil
Trimay® Wear Plate T157 Iron-based Steel Overlay
Overlay Description: T157 is a iron-based steel overlay wear solution with a unique proprietary chemical composition designed to withstand heavy wear environments exposed to mild-moderate direct imp..