Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 4320 microns | 170 mil | Sheet; Internal |
Azdel Plus C327-B01 31% Chopped Fiber Mat / PP Resin Matrix AZDEL® C327-B01 is a glass mat thermoplastic laminate based upon a random oriented chopped fiber mat contained within a polypropylene resin matrix. This composite material features high flow prope.. |