Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 1450 - 1600 microns | 57.0 - 63.0 mil | Overall |
Arlon 25122R060 0.060" (1.52 mm) Silicone Rubber on Laminated Fluoropolymer Film Appearance: Red silicone rubber chemically bonded to fluoropolymer filmThis data represents typical values for the production material. The data should not be used to write, or in place of, material.. |
|||
Thickness | 1450 - 1600 microns | 57.0 - 63.0 mil | Overall |
Arlon LW6015Xxx-P0 0.060" (1.52 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) with Poly Interleave Design/Construction: Triangular Cross Section Fusible TapeArlon LevelWrap® Tape: LevelWrap® has tapered edges and a colored line along its apes. The purpose of the line is to act as a guide for su.. |
|||
Thickness | 1450 - 1700 microns | 57.0 - 67.0 mil | Overall |
Arlon R30651R062 0.062" (1.57 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place .. |
|||
Thickness | 1450 - 1700 microns | 57.0 - 67.0 mil | Overall |
Arlon R34482X062 0.062" (0.356 mm) Uncured/Cured Silicone Rubber Design/Construction:Side 1: Cured/Post-cured Unsupported Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of, materi.. |
|||
Thickness | 1450 - 1700 microns | 57.0 - 67.0 mil | Side 1 |
Arlon R34482X062 0.062" (0.356 mm) Uncured/Cured Silicone Rubber Design/Construction:Side 1: Cured/Post-cured Unsupported Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of, materi.. |