Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 290 - 350 microns | 11.4 - 13.8 mil | |
Beijing Evergrow Resources ASHRAE HEPA ULPA-K49 Glass Fiber Paper Fiber made from melted glass that is drawn into a thin fiber less than a thousandth of an inch in diameter. The fiber may be spun into threads and woven into fabrics which suitable for many applicat.. |
|||
Thickness | 290 - 350 microns | 11.4 - 13.8 mil | |
Beijing Evergrow Resources ASHRAE HEPA ULPA-K19 Glass Fiber Paper Fiber made from melted glass that is drawn into a thin fiber less than a thousandth of an inch in diameter. The fiber may be spun into threads and woven into fabrics which suitable for many applicat.. |
|||
Thickness | 290 - 350 microns | 11.4 - 13.8 mil | |
Beijing Evergrow Resources ASHRAE HEPA ULPA-K29 Glass Fiber Paper Fiber made from melted glass that is drawn into a thin fiber less than a thousandth of an inch in diameter. The fiber may be spun into threads and woven into fabrics which suitable for many applicat.. |
|||
Thickness | 290 - 350 microns | 11.4 - 13.8 mil | |
Beijing Evergrow Resources ASHRAE HEPA ULPA-K39 Glass Fiber Paper Fiber made from melted glass that is drawn into a thin fiber less than a thousandth of an inch in diameter. The fiber may be spun into threads and woven into fabrics which suitable for many applicat.. |
|||
Thickness | 290 - 350 microns | 11.4 - 13.8 mil | |
Beijing Evergrow Resources ASHRAE HEPA ULPA-K59 Glass Fiber Paper Fiber made from melted glass that is drawn into a thin fiber less than a thousandth of an inch in diameter. The fiber may be spun into threads and woven into fabrics which suitable for many applicat.. |