Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 348 microns | 13.7 mil | |
Hexcel® HexForce™ AGP370-8H Carbon Fabric Hexcel's carbon fibers contain high strength-to-weight and stiffness-to-weight ratios. Carbon fabrics are thermally and electrically conductive and exhibit excellent fatigue resistance. When proper.. |