Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 3150 microns | 124 mil | Standard; Laminate |
GrafTech GRAFOIL® GHE Standard Fluid Sealing Laminate, Metal Reinforced GRAFOIL® Grade GHE laminate is made with GTB flexible graphite mechanically bonded to both faces of a 316 or 316L stainless steel tang metal insert. Surface identifiable, the laminate is branded .. |
|||
Thickness | 3160 microns | 124 mil | |
SMAC SMACFOAM® 1250S-02 Damping Material SMAC has developed sound absorbing material dedicated to be used in aerospace and defense activities thanks to its good acoustic properties, its lightweight and its fire resistance properties.Uses: .. |