Physical Properties Metric English Comments
Thickness 1200 - 1800 microns
47.2 - 70.9 mil
Standard
Parker Chomerics WIN-SHIELD™ Elite EMI Shielded Window
Description: Shielded Windows WIN-SHIELD™ EMI shielded windows provide exceptional optical performance without sacrificing EMI shielding. This new generation of shielded windows is designed specif..
Thickness 1200 microns
47.2 mil
SMAC SMACWRAP® EX Damping Material, 0.12 mm
SMACWRAP® concept is a smart and lightweight solution to embed into composite structures a very thin viscoelastic material. The SMACWRAP® will then bring damping to the composite structure wit..
Thickness 1200 microns
47.2 mil
Zoltek Pyron® Satin Weave & Knit Fabric Oxidized Pan Fiber
Oxidized Pan Fiber