Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 200 - 3000 microns | 7.87 - 118.1 mil | <1±0.03 :: 1-1.5±0.05 :: >1.5±0.6 |
Sinotek Materials B Graphite Sheet Flexible Graphite Sheet/Roll is made from expanding Expandable Graphite under high temperature and then rolling. It has the characteristics of high temperature resistance, corrosion resistance and g.. |
|||
Thickness | 200 - 3000 microns | 7.87 - 118.1 mil | <1±0.03 :: 1-1.5±0.05 :: >1.5±0.5 |
Sinotek Materials A Graphite Sheet Flexible Graphite Sheet/Roll is made from expanding Expandable Graphite under high temperature and then rolling. It has the characteristics of high temperature resistance, corrosion resistance and g.. |
|||
Thickness | 200 - 3000 microns | 7.87 - 118.1 mil | <1±0.03 :: 1-1.5±0.05 :: >1.5±0.7 |
Sinotek Materials C Graphite Sheet Flexible Graphite Sheet/Roll is made from expanding Expandable Graphite under high temperature and then rolling. It has the characteristics of high temperature resistance, corrosion resistance and g.. |