Physical Properties Metric English Comments
Thickness 2970 microns
117 mil
Thickness of film tested; ASTM D374
Eastman Tritan GX100 Copolyester
Eastman Tritan copolyester GX100's strength, clarity and temperature resistance make it ideal for demanding applications. Extruded Sheet is manufactured with Eastman's Tritan copolyester GX100 resi..