Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 295 microns | 11.6 mil | |
Hexcel® HexForce™ TEF7 Specialty Fabric Hexcel features custom fabric design and manufacturing. We tailor our customers' reinforcement fabrics for optimum performance. We are able to combine two or more different fibers (carbon, glass, a.. |
|||
Thickness | 295 microns | 11.6 mil | Typical; ASTM D374 |
DuPont™ Nomex® E56 Paper, 12 mil Nominal Thickness Nomex® Type E56 is designed for cost critical uses which require lesser amounts of mechanical and electrical strength than other Nomex® grades. It is thermally similar to Nomex® Type 410 but as.. |