Polymer Property : Thickness = 10.4 mil Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Thickness 264 microns
10.4 mil
Hexcel® HexForce™ 6581 Fiber Glass Fabric
Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential ..
Thickness 264 microns
10.4 mil
Hexcel® HexForce™ GA060 Carbon Fabric
Hexcel's carbon fibers contain high strength-to-weight and stiffness-to-weight ratios. Carbon fabrics are thermally and electrically conductive and exhibit excellent fatigue resistance. When proper..
Thickness 264 microns
10.4 mil
Total; ASTM D3652
3M 472 Vinyl Tape
3M™ Vinyl Tape 472 is comprised of a heavy duty backing with a black pigmented rubber adhesive. The thick vinyl backing makes it ideal for applications requiring both abrasion resistance and the in..