Physical Properties Metric English Comments
Thickness 262 microns
10.3 mil
Hexcel® HexForce™ 1629 Aramid Fabric
Hexcel manufactures aramid fabrics for use in aerospace applications as well as marine, tooling and recreational products where high strength, low weight, and impact resistance are essential. Aramid..