Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 36.3 microns | 1.43 mil | Backing; ASTM D3652 |
3M Scotch® 5912 Cellophane Tape Scotch® Tape 5972 is a transparent cellophane tape designed for light-duty packaging applications. It is typically used for bag closing, temporary holding, and L-clip applications that do not put s.. |
|||
Thickness | 36.3 microns | 1.43 mil | Backing; ASTM D3652 |
3M Scotch® 610 Cellophane Film Tape Scotch® Cellophane Film Tape 610 is a high performance, transparent cellophane film tape featuring a high tack adhesive system. This product offers excellent adhesion, dispensing and handling prope.. |