Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 24.0 microns | 0.945 mil | Cured, Printed through 230 stainless steel mesh with 13 micron emulsion |
Gwent Electronic Materials C2050517D1 Carbon Graphite Ink This is designed for screen-printing of working electrodes for electrochemical sensors. The paste is highly thixotropic which gives it very good definition on printing. This product has been design.. |