Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 23.0 microns | 0.906 mil | when printed through a 156 mesh |
Gwent Electronic Materials C2000215D4 Silver / Silver Chloride Paste C2000215D4 has a ratio of Silver to Silver Chloride of 50/50. This is used for reference electrodes in Medical Diagnostics, Environmental Sensor and the "Agri-Food" Industries. It forms part of a .. |
|||
Thickness | 23.0 microns | 0.906 mil | Cured film on glass |
Gwent Electronic Materials C2090819P2 Silver Ink This product is part of a range of Heat Curable Inks designed specifically for use in Photovoltaic panels. These products are based on a unique curing process that results in the low temperature fo.. |
|||
Thickness | 23.0 microns | 0.906 mil | Wet Recommended Film |
Chesterton 775 Moisture Shield Description: Chesterton® 775 Moisture Shield is a moisture displacing, clear protective coating that protects parts and equipment from corrosion for months. Sprayed on bare metal, it leaves a lubri.. |
|||
Thickness | 23.0 microns | 0.906 mil | Critical Film Thickness; AGFP Method |
Asahi Glass Fluon® XAD912 PTFE Aqueous Dispersion Fluon®PTFE aqueous dispersions are useful for glass cloth coating, metal coating, binder, additive in resin, feedstock of heat resistive paint ,etc.Information provided by Asahi Glass Company, Inc... |