Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 21.6 microns | 0.850 mil | Nominal; ExxonMobil Method |
ExxonMobil Bicor® 85 LTSC OPP Film Product Description: Bicor LTSC is a two-side coated OPP film which is designed for use in high-speed or demanding horizontal, fin seal, packaging applications. The low-temperature seal coating (LTS.. |