Polymer Property : Thickness = 0.820 microns Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Thickness 0.820 microns
0.0323 mil
3000 rpm
Dow SiLK™ I 820 Semiconductor Dielectric Resin
SiLK™ I 820 is designed for easy integration and extendibility, and its formulations offer a robust feature set. High thermal stability and fracture toughness means SilK™ I 820 is compatible with..