Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 1.02 - 17.8 microns | 0.0400 - 0.700 mil | Possible range |
XADC-Armoloy Armoloy® TDC Hard Chromium Coating ARMOLOY® TDC is a low temperature, multi-state surface finishing process. ARMOLOY® utilizes proprietary chemical solutions and application processes that are carefully monitored to produce it.. |
|||
Thickness | 1.02 - 17.8 microns | 0.0400 - 0.700 mil | Possible range |
XADC-Armoloy Diamond-Chrome Composite Coating XADC-Armoloy® combines the Armoloy® TDC chromium coating with spherical diamond particulates. The XADC-Armoloy® coating enhances the durability of components used in a wide range of applications.. |