Polymer Property : Thickness = 0.350 mil Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Thickness 8.89 microns
0.350 mil
Chengdu Polyster 100 LPI Lenticular Lens Sheet, APET
Good for ink adhesion. The image is sharp and clear. It is specially designed for advertisement and packaging with high definition and clearness requirement. The suitable graphic effects: flip, 3D, ..