Polymer Property : Thickness = 0.330 microns Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Thickness 0.240 - 0.330 microns
0.00945 - 0.0130 mil
Dow Corning FOX® PMCP22 Flowable Oxide
Spin-on dielectric (HSQ)Information provided by Dow Corning