Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 0.229 microns | 0.00900 mil | cured laminate, per ply |
Park Electrochemical Nelcote® V-376 Cyanate Ester Epoxy Prepregs, 7781 E-Glass Reinforced Nelcote® V-376 is a Cyanate Ester matrix providing excellent electrical and mechanical properties for harsh aircraft, shipboard, and undersea applications for Radomes, Antenna, and Reflectors. Simp.. |