Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 4.62 microns | 0.182 mil | ASTM D3652 |
3M Scotch® 2380 Performance Masking Tape Scotch® Performance Masking Tape 2380 is a smooth, strong, mini-crepe paper masking tape suitable for most paint masking applications.Information provided by 3M |