Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 1.30 - 1.84 microns | 0.0512 - 0.0724 mil | 2000-4000 rpm |
Dow SiLK™ I 1500 Semiconductor Dielectric Resin SiLK™ I 1500 is designed for easy integration and extendibility, and its formulations offer a robust feature set. High thermal stability and fracture toughness means SilK™ I 1500 is compatible wi.. |