Polymer Property : Pellet Density = 0.330 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Pellet Density 0.330 - 0.370 g/cc
0.0119 - 0.0134 lb/in³
ASTM D2840
Trelleborg AEM Eccospheres® IG-101 Sodium Borosilicate Glass Microspheres
Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific..
Pellet Density 0.330 - 0.370 g/cc
0.0119 - 0.0134 lb/in³
ASTM D2840
Trelleborg AEM Eccospheres® SI-350 Sodium Borosilicate Glass Microspheres
Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific..
Pellet Density 0.330 - 0.370 g/cc
0.0119 - 0.0134 lb/in³
ASTM D2840
Trelleborg AEM Eccospheres® SID-350Z Sodium Borosilicate Glass Microspheres
Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific..