Physical Properties | Metric | English | Comments |
---|---|---|---|
Cell Length | 0.600 - 1.20 mm | 0.0236 - 0.0472 in | |
Zotefoams Evazote® EV120CN Conductive Ethylene Vinyl Acetate Copolymer Foam Evazote® is a closed cell, cross-linked EVA copolymer foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outsta.. |
|||
Cell Length | 0.500 - 1.20 mm | 0.0197 - 0.0472 in | |
Zotefoams Plastazote® HL47 Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Cell Length | 0.600 - 1.20 mm | 0.0236 - 0.0472 in | |
Zotefoams Plastazote® LD14IC Low Density Polyethylene Foam, Intermediate Cell Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Cell Length | 0.600 - 1.20 mm | 0.0236 - 0.0472 in | |
Zotefoams Plastazote® LD15IC Low Density Polyethylene Foam, Intermediate Cell Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |