Physical Properties | Metric | English | Comments |
---|---|---|---|
Cell Length | 0.380 mm | 0.0150 in | Typical Diameter |
Zotefoams Plastazote® LD15 Low Density Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |