Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.100 - 96.0 g/10 min | 0.100 - 96.0 g/10 min | Average value: 20.7 g/10 min Grade Count:28 |
Overview of materials for Polyphenylene Ether, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Molded". Each property range of values reported is minimum and maximum values of ap.. |