Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 95.9 g/10 min @Load 10.0 kg, Temperature 360 °C |
95.9 g/10 min @Load 22.0 lb, Temperature 680 °F |
ISO 1133 |
BASF Ultrason® E 2010 MR SW 10111 PESU Description: Unreinforced, medium viscosity standard injection molding grade, demolding optimized. Abbreviated designation according to ISO 1043-1: PESU.Information provided by BASF |
|||
Melt Flow | 95.9 g/10 min @Load 10.0 kg, Temperature 360 °C |
95.9 g/10 min @Load 22.0 lb, Temperature 680 °F |
ISO 1133 |
BASF Ultrason® E 2010 HC PESU Information provided by BASF |
|||
Melt Flow | 95.9 g/10 min @Load 10.0 kg, Temperature 360 °C |
95.9 g/10 min @Load 22.0 lb, Temperature 680 °F |
ISO 1133 |
BASF Ultrason® E 2010 SW Q31 10088 PESU Information provided by BASF |