Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 2.00 - 93.8 g/10 min | 2.00 - 93.8 g/10 min | Average value: 17.8 g/10 min Grade Count:15 |
Overview of materials for Nylon 6, 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. .. |