Physical Properties Metric English Comments
Melt Flow 93.8 g/10 min

@Load 5.00 kg,
Temperature 275 °C
93.8 g/10 min

@Load 11.0 lb,
Temperature 527 °F
ISO 1133
BASF Ultramid® B3GK24 10/20% Glass Bead/Fiber Filled PA6 (Dry)
Ultramid B3GK24 is 30% combined glass-fiber and glass bead injection molding PA6 grade for industrial articles having very high dimensional stability.
Melt Flow 93.8 g/10 min

@Load 5.00 kg,
Temperature 275 °C
93.8 g/10 min

@Load 11.0 lb,
Temperature 527 °F
ISO 1133
BASF Ultramid® B3GK24 10/20% Glass Bead/Fiber Filled PA6 (Conditioned)
Ultramid B3GK24 is 30% combined glass-fiber and glass bead injection molding PA6 grade for industrial articles having very high dimensional stability.
Melt Flow 93.8 g/10 min

@Load 5.00 kg,
Temperature 275 °C
93.8 g/10 min

@Load 11.0 lb,
Temperature 527 °F
ISO 1133
BASF Ultramid® B3GK24 BK 00564 10/20% Glass/Glass Bead Filled PA6 (Conditioned)
Description: combined 10% glass-fiber and 20% glass-bead reinforced injection-molding grade for technical articles of very good dimensional stability, for instance, vehicle ash tray housings and ele..
Melt Flow 93.8 g/10 min

@Load 5.00 kg,
Temperature 275 °C
93.8 g/10 min

@Load 11.0 lb,
Temperature 527 °F
ISO 1133
BASF Ultramid® B3GK24 BK 00564 10/20% Glass/Glass Bead Filled PA6 (Dry)
Description: combined 10% glass-fiber and 20% glass-bead reinforced injection-molding grade for technical articles of very good dimensional stability, for instance, vehicle ash tray housings and ele..