Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 9.8 g/10 min | 9.8 g/10 min | ISO 1133:1997 |
Nanocyl PLASTICYL™ PP2001 Polypropylene with 1 wt% Multi-Wall Carbon Nanotubes PLASTICYL™ is a family of Multi-Wall Carbon Nanotube (MWNT) thermoplastic concentrates for applications requiring superior electrical conductivity and electrostatic discharge (ESD) properties. PLA.. |
|||
Melt Flow | 9.8 - 10.8 g/10 min @Load 1.20 kg, Temperature 250 °C |
9.8 - 10.8 g/10 min @Load 2.65 lb, Temperature 482 °F |
|
Kazanorgsintez PC-075 Polycarbonate Production Method: Obtained by means of polycondensation method. Application: Intended for manufacture of optical products by method of die-casting (including CD, DVD, and other discs), as well .. |
|||
Melt Flow | 9.8 g/10 min @Load 10.0 kg, Temperature 220 °C |
9.8 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® SD-0190H ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 9.8 g/10 min @Load 10.0 kg, Temperature 220 °C |
9.8 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® SD-0190H ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 9.8 g/10 min @Load 5.00 kg, Temperature 280 °C |
9.8 g/10 min @Load 11.0 lb, Temperature 536 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL NH5020 PPE+PS Noryl* NH5020 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated flame reta.. |
|||
Melt Flow | 9.8 g/10 min @Load 5.00 kg, Temperature 280 °C |
9.8 g/10 min @Load 11.0 lb, Temperature 536 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL NH5020 PPE+PS (Asia Pacific) Noryl* NH5020 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated flame reta.. |
|||
Melt Flow | 9.8 g/10 min @Load 5.00 kg, Temperature 280 °C |
9.8 g/10 min @Load 11.0 lb, Temperature 536 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL NH5020 PPE+PS (Europe-Africa-Middle East) Noryl* NH5020 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated flame reta.. |
|||
Melt Flow | 9.8 g/10 min @Load 2.16 kg, Temperature 190 °C |
9.8 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
BASF Ultraform® N2520 L POM Description: Is a POM, product having reduced electric surface resistance.Information provided by BASF |